  • 90/10 Copper Nickel UNS C96200
    Product Code: 49019

    90/10 Copper Nickel UNS C96200

    Copper-nickel 90/10 (86.85% Cu, 10% Ni) per CDA C96200 for seawater corrosion resistance and marine piping applications. 2-20 ingot.
    Lead-free
    Lead-Free Marine Grade Seawater Corrosion Resistant Stress Corrosion Cracking Resistant
    Solidus
    2,010°F (1,099°C)
    Liquidus
    2,100°F (1,149°C)
    Density
    0.323 lbs/in³ (8.94 g/cm³)
    Primary Elements
    Cb, Cu, Fe, Mn, Ni
    Nominal Composition
    0.75% Cb, 1% Mn, 1.4% Fe, 10% Ni, 86.85% Cu
    Shapes
    Ingot
  • Lead Sounding Weights
    Product Code: 5003

    Lead Sounding Weights

    Lead sounding weights in 7 lb size for marine depth measurement counterweighting and corrosion-resistant ballast applications.
    7 lb Standard Size Marine Depth Measurement Seawater Corrosion Resistant Sediment Sampling
    Solidus
    621°F (327°C)
    Liquidus
    621°F (327°C)
    Density
    0.41 lbs/in³ (11.34 g/cm³)
    Primary Elements
    Pb
    Nominal Composition
    Bal, 95.5% Pb
    Shapes
    Bricks, Shot
  • Navy G Bronze Alloy UNS C90300
    Product Code: 4884

    Navy G Bronze Alloy UNS C90300

    Navy G bronze (88% Cu, 4% Zn, 8% Sn) per CDA C90300 for steam pressure and marine applications up to...
    Lead-Free Marine Grade Seawater Corrosion Resistant Steam Pressure Rated
    Solidus
    1,570°F (854°C)
    Liquidus
    1,832°F (1,000°C)
    Density
    0.318 lbs/in³ (8.8 g/cm³)
    Primary Elements
    Zn, Cu, Sn
    Nominal Composition
    4% Zn, 8% Sn, 88% Cu
    Shapes
    Ingot