  • Product code: 892NJ1

    Spin Cast Zinc Alloy - J1

    Lead-free Proprietary Grain RefinersThin Cross Section CastingLead-Free CertifiedHigh Compressive Strength
    Lead-free zinc spin cast alloy with grain refiners in 4-20 lb KZ ingot form. Liquidus 734F, pouring temp 850-950F. For thin cross sections and maximum detail.
    Liquidus
    734°F (390°C)
    Density
    0.24 lbs/in³ (6.64 g/cm³)
    Primary Elements
    Zn · Cu · Al · Mg · Ti
  • Product code: 892NS1

    Spin Cast Zinc Alloy - S1

    Lead-free Original Kor-Zee FormulationThick Cross Section GradeLead-FreeGrain Refined
    Original lead-free zinc spin cast alloy in 4-20 lb KZ ingot form. Liquidus 734F, pouring temp 800-875F. For thick cross section spin cast mold applications.
    Liquidus
    734°F (390°C)
    Density
    0.244 lbs/in³ (6.75 g/cm³)
    Primary Elements
    Zn · Cu · Al · Mg · Ti
  • Product code: 8934A

    Superdie I / Zamak 2 Zinc Base Alloy

    Lead-free Easy CastabilityHigh DuctilityRubber Mold CompatibleSculpture and Die Casting
    Zinc-base rubber mold casting alloy in 4-20 lb ingot form. Easy to cast and highly ductile. Used for die casting and sculpture applications.
    Solidus
    715°F (379°C)
    Liquidus
    735°F (391°C)
    Density
    0.24 lbs/in³ (6.6 g/cm³)
    Primary Elements
    Zn · Al · Cu
  • Product code: 7007

    SW Grade Tin

    Lead-free Controlled Particle Size DistributionHigh Sintering EfficiencyAerospace PM GradeFriction Material Additive
    High-purity SW grade tin powder. Melting point 449.5°F (231.9°C). Used for sintered components, friction materials, tin compound synthesis, and aerospace/electronics powder metallurgy.
    Solidus
    449°F (232°C)
    Liquidus
    450°F (232°C)
    Density
    0.264 lbs/in³ (7.31 g/cm³)
    Primary Elements
    Sn
  • Product code: 79010

    Tin Base Level Alloy 1

    Optimized for Flat Polished SurfacesCadmium Microstructure RefinementPlaque and Medallion GradeExtended Mold Life
    Tin-lead-antimony-cadmium pewter (90% Sn, 6% Pb, 2% Sb, 2% Cd) for castings with flat polished surfaces. Low melting point extends mold life.
    Solidus
    266°F (130°C)
    Liquidus
    329°F (165°C)
    Density
    0.287 lbs/in³ (7.94 g/cm³)
    Primary Elements
    Sn · Pb · Sb · Cd
  • Product code: 2581

    TRU Alloy, 281 F, 138 C Eutectic Low Melting Alloy

    Lead-free Eutectic CompositionMinimal Volume Change on SolidificationLead-FreeAerospace Fixturing
    Binary eutectic fusible alloy, 58% Bi / 42% Sn. Melting point 281°F (138°C). Lead-free. Used for jet engine blade fixturing, foundry patterns, and fusible safety elements.
    Solidus
    281°F (138°C)
    Liquidus
    281°F (138°C)
    Density
    0.309 lbs/in³ (8.72 g/cm³)
    Primary Elements
    Bi · Sn
  • Product code: L2

    Tuftex 4X Alloy

    Proprietary Lead-Base BabbittLow-Speed Bearing ApplicationsGood EmbeddabilityJackson Wheeler Formulation
    Proprietary lead-base Babbitt alloy for low-speed bearing applications. Forms: ingot.
    Solidus
    473°F (245°C)
    Liquidus
    509°F (265°C)
    Density
    0.383 lbs/in³ (10.6 g/cm³)
    Primary Elements
    Pb · Sb · Sn
  • Product code: C3

    Tuftex Chipper Alloy

    Proprietary Lead-BaseWood Chipper Knife ApplicationImpact and Wear ResistanceJackson Wheeler Formulation
    Proprietary lead-base alloy for wood chipper knife manufacturing. Forms: ingot.
    Solidus
    469°F (243°C)
    Liquidus
    484°F (251°C)
    Density
    0.375 lbs/in³ (10.37 g/cm³)
    Primary Elements
    Pb · Sb · Sn · Ni · Cu
  • Product code: J1

    Tuftex Duratex Alloy

    Nickel-Modified Lead-Base BabbittIncreased HardnessHigher Load Capacity Than Standard Lead BabbittJackson Wheeler Proprietary
    Proprietary lead-base alloy with nickel addition for increased hardness. Forms: ingot.
    Solidus
    462°F (239°C)
    Liquidus
    487°F (253°C)
    Density
    0.361 lbs/in³ (10 g/cm³)
    Primary Elements
    Pb · Sb · Sn · Ni · Cu
  • Product code: P1

    Tuftex Gib Shoe Alloy

    Elevator Gib Shoe ApplicationProprietary Lead-Base BabbittGuide Rail ConformabilityJackson Wheeler Formulation
    Proprietary lead-base Babbitt for elevator bearing relining applications. Forms: ingot.
    Solidus
    464°F (240°C)
    Liquidus
    500°F (260°C)
    Density
    0.363 lbs/in³ (10.04 g/cm³)
    Primary Elements
    Pb · Sb · Sn · Ni · Cu