Zinc

Sort By:

Showing 8 of 258 products

  • 711.1 Aluminum Alloy

    Lead-free Natural Aging (No Heat Treatment)Excellent BrazabilitySuperior Dimensional Stability
    Al-Zn casting alloy (91.7% Al, 6.5% Zn) with natural aging strength and excellent brazability. No heat treatment required. 3-16 lb ingot.
    Solidus
    1,100°F (593°C)
    Liquidus
    1,195°F (646°C)
    Density
    0.102 lbs/in³ (2.82 g/cm³)
    Primary Elements
    Al · Zn · Fe
  • Product code: 8995

    99/1 Zinc Aluminum Solder

    Lead-free Musical Instrument GradeCorrosion-Resistant Zinc AlloyLong Historical UseHardware and Architectural Applications
    Zinc-aluminum solder alloy (99% Zn, 1% Al) for metal joining in musical instruments, hardware, and corrosion-resistant applications. 4-20 lb ingot.
    Solidus
    720°F (382°C)
    Liquidus
    774°F (412°C)
    Density
    0.254 lbs/in³ (7.02 g/cm³)
    Primary Elements
    Zn · Al
  • Product code: 5731

    25% Tin Pewter Alloy

    Lowest Cost Pewter-Type AlloyHigh Lead ContentDecorative Casting GradeHigh Density for Weight Applications
    Low-cost lead-tin pewter alloy (74% Pb, 24% Sn, 2% Sb) in 5-8 lb ingot for inexpensive end-use decorative castings where high weight is acceptable.
    Solidus
    361°F (183°C)
    Liquidus
    520°F (271°C)
    Density
    0.287 lbs/in³ (7.95 g/cm³)
    Primary Elements
    Pb · Sn · Sb
  • Product code: 78821

    ASTM B-23 Grade 11 Babbitt

    ASTM B-23 Grade 11 Heavy-Load Bearing GradeHigh HardnessTin-Base
    Tin-base babbitt (87.5% Sn, 6.75% Sb, 5.75% Cu) per ASTM B-23 Grade 11 for heavy-load bearing applications. Wire and ingot forms.
    Solidus
    468°F (242°C)
    Liquidus
    669°F (354°C)
    Density
    0.266 lbs/in³ (7.35 g/cm³)
    Primary Elements
    Sn · Sb · Cu
  • C355.2 Aluminum Alloy

    Lead-free Superior Pressure TightnessHigh Fatigue StrengthHigh-Purity GradeAerospace Grade
    High-purity Al-Si-Cu-Mg casting alloy (93% Al, 5% Si, 1% Cu) with superior pressure tightness and fatigue strength. Aerospace grade. 30 lb ingot.
    Solidus
    1,015°F (546°C)
    Liquidus
    1,150°F (621°C)
    Density
    0.098 lbs/in³ (2.71 g/cm³)
    Primary Elements
    Al · Si · Cu · Mg
  • Product code: 4992

    Beryllium Copper 70C

    Lead-free Highest Copper Content BeCu GradeSuperior Thermal ConductivityInvestment and Centrifugal CastingSuperior Strength and Hardness
    Highest-copper BeCu alloy with superior strength; hardness; and thermal conductivity. Recommended for investment; continuous; and centrifugal casting. Forms: 2-5 lb ingot.
    Solidus
    1,950°F (1,066°C)
    Liquidus
    2,000°F (1,093°C)
    Density
    0.318 lbs/in³ (8.81 g/cm³)
    Primary Elements
    Cu · Cr · Be
  • Product code: J1

    Tuftex Duratex Alloy

    Nickel-Modified Lead-Base BabbittIncreased HardnessHigher Load Capacity Than Standard Lead BabbittJackson Wheeler Proprietary
    Proprietary lead-base alloy with nickel addition for increased hardness. Forms: ingot.
    Solidus
    462°F (239°C)
    Liquidus
    487°F (253°C)
    Density
    0.361 lbs/in³ (10 g/cm³)
    Primary Elements
    Pb · Sb · Sn · Ni · Cu
  • Product code: W1

    Tuftin Duratin

    Tin-Base BabbittMedium Load ApplicationsHigher Strength Than Lead BabbittJackson Wheeler Formulation
    Proprietary tin-base Babbitt alloy for medium load bearing applications. Forms: ingot.
    Solidus
    363°F (184°C)
    Liquidus
    491°F (255°C)
    Density
    0.285 lbs/in³ (7.88 g/cm³)
    Primary Elements
    Pb · Sb · Sn · Ni · Cu · Te

Showing 251–258 of 258 resultsSorted by popularity