  • Tuftex Gib Shoe Alloy
    Product Code: P1

    Tuftex Gib Shoe Alloy

    Proprietary lead-base Babbitt for elevator bearing relining applications. Forms: ingot.
    Elevator Gib Shoe Application Proprietary Lead-Base Babbitt Guide Rail Conformability Jackson Wheeler Formulation
    Solidus
    464°F (240°C)
    Liquidus
    500°F (260°C)
    Density
    0.363 lbs/in³ (10.04 g/cm³)
    Primary Elements
    Pb · Sb · Sn · Ni · Cu
    Nominal Composition
    Proprietary
  • Tuftex Lubrite
    Product Code: A4

    Tuftex Lubrite

    Proprietary Jackson Wheeler Tuftex bearing alloy. Forms: ingot. Contact Belmont Metals for application details.
    Proprietary Tuftex Bearing Alloy Jackson Wheeler Formulation Industrial Bearing Application Contact Belmont for Details
    Solidus
    464°F (240°C)
    Liquidus
    500°F (260°C)
    Density
    0.365 lbs/in³ (10.11 g/cm³)
    Primary Elements
    Pb · Sb · Sn · Ni · Cu · Te
    Nominal Composition
    Proprietary
  • Tuftin Hercules Genuine
    Product Code: D3

    Tuftin Hercules Genuine

    Proprietary tin-base Babbitt alloy for high-speed; high-load bearing applications. Forms: ingot.
    Tin-Base Babbitt High-Speed High-Load Applications Premium Performance Jackson Wheeler Proprietary
    Solidus
    363°F (184°C)
    Liquidus
    500°F (260°C)
    Density
    0.319 lbs/in³ (8.83 g/cm³)
    Primary Elements
    Pb · Sb · Sn · Ni · Cu · Te
    Nominal Composition
    Proprietary