Lowest Pouring Temperature BeCu

Filter By

Filters
Melting Point (Solidus), °F

Melting Point (Solidus), °F: 1625 — 1625

Density, lbs/in³

Density, lbs/in³: 0 — 1

Lead Free
See more See less
Custom Request
Can't find the right composition?
Get Expert Help

Sort By:

  • Beryllium Copper 275C UNS C82800
    Product Code: 4971

    Beryllium Copper 275C UNS C82800

    Highest-strength BeCu alloy UNS C82800 with maximum hardness; wear resistance; and fluidity. Lowest pouring temperature of BeCu alloys. Forms: shot...
    Lead-free
    Highest Strength and Hardness BeCu Grade Lowest Pouring Temperature BeCu Excellent Wear Resistance
    Solidus
    1,625°F (885°C)
    Liquidus
    1,710°F (932°C)
    Density
    0.292 lbs/in³ (8.09 g/cm³)
    Primary Elements
    Cu · Be · Co · Si · Ti
    Nominal Composition
    0.07% Ti, 0.3% Si, 0.5% Co, 2.7% Be, 96.43% Cu

Showing the single result