  • A357.2 Aluminum Alloy

    A357.2 Aluminum Alloy

    High-strength Al-Si-Mg casting alloy (92.2% Al, 7% Si, 0.6% Mg) with excellent pressure tightness. Heat treatable. 30 lb ingot.
    Lead-free
    High Strength Excellent Pressure Tightness Heat Treatable
    Solidus
    1,035°F (557°C)
    Liquidus
    1,135°F (613°C)
    Density
    0.097 lbs/in³ (2.68 g/cm³)
    Primary Elements
    Al · Si · Mg
    Nominal Composition
    0.6% Mg, 7% Si, 92.2%Al, Bal
  • A444.2 Aluminum Alloy

    A444.2 Aluminum Alloy

    High-ductility Al-Si alloy (93% Al, 7% Si) with low iron for maximum elongation and impact resistance. Safety-critical casting grade. 3-16...
    Lead-free
    High Ductility Excellent Impact Resistance Low Iron Superior Weldability
    Solidus
    1,065°F (574°C)
    Liquidus
    1,135°F (613°C)
    Density
    0.097 lbs/in³ (2.68 g/cm³)
    Primary Elements
    Al · Si
    Nominal Composition
    7% Si, 93% Al
  • C357.2 Aluminum Alloy

    C357.2 Aluminum Alloy

    High-purity Al-Si-Mg casting alloy (92.22% Al, 7% Si, 0.6% Mg) with exceptional fracture toughness. Safety-critical aerospace grade. ~35 lb ingot.
    Lead-free
    High-Purity Grade Exceptional Fracture Toughness Aerospace Grade Superior Corrosion Resistance
    Solidus
    1,035°F (557°C)
    Liquidus
    1,135°F (613°C)
    Density
    0.097 lbs/in³ (2.68 g/cm³)
    Primary Elements
    Al · Si · Mg
    Nominal Composition
    0.6% Mg, 7% Si, 92.22% Al, Bal
  • F357 Aluminum Alloy (Beryllium-Free A357)

    F357 Aluminum Alloy (Beryllium-Free A357)

    Beryllium-free Al-Si-Mg alloy (6.5–7.5% Si, 0.45–0.7% Mg, Be <0.002%) optimized for additive manufacturing and investment casting. 3-16 ingot.
    Lead-free
    Beryllium-Free Additive Manufacturing Optimized Superior Fatigue Resistance Investment Casting Grade
    Solidus
    1,035°F (557°C)
    Liquidus
    1,135°F (613°C)
    Density
    0.097 lbs/in³ (2.68 g/cm³)
    Primary Elements
    Al · Si · Mg · Ti
    Nominal Composition
    Aluminum: Balance, Beryllium: <0.002% (Max), Magnesium: 0.45 - 0.7%, Silicon: 6.5 - 7.5%, Titanium: 0.04 - 0.2%