Find the Right Alloy for Your Application

Sort By:

Showing 10 of 225 products

  • Product code: 1907

    10% Cobalt Aluminum

    Lead-free Creep ResistanceHigh-Temperature StrengthIron Phase Modifier
    Al-Co master alloy (90% Al, 10% Co) for precise cobalt additions to improve high-temperature strength and creep resistance. 1" x 6" x 12" slabs.
    Solidus filter
    1,250°F (677°C)
    Liquidus
    2,050°F (1,121°C)
    Density
    0.158 lbs/in³ (4.37 g/cm³)
    Primary Elements
    Al · Co
  • Product code: 4907

    10% Cobalt Copper

    Lead-free Controlled Cobalt AdditionCorrosion Resistance ImproverJewelry Alloy AdditionJewelry and Foundry Grade
    Cobalt copper master alloy (90% Cu, 10% Co) for corrosion resistance improvement in copper alloys. Shot form for jewelry and foundry additions.
    Solidus filter
    1,994°F (1,090°C)
    Liquidus
    2,102°F (1,150°C)
    Density
    0.323 lbs/in³ (8.95 g/cm³)
    Primary Elements
    Co · Cu
  • Product code: 19013

    10% Ferro Aluminum

    Lead-free Controlled Iron AdditionDie Soldering PreventionLow LiquidusRapid Dissolution
    Al-Fe master alloy (90% Al, 10% Fe) for controlled iron additions to aluminum melts. Low liquidus for easy dissolution. 16-20 waffle.
    Solidus filter
    1,211°F (655°C)
    Liquidus
    1,565°F (852°C)
    Density
    0.103 lbs/in³ (2.85 g/cm³)
    Primary Elements
    Al · Fe
  • Product code: 49011

    10% Zirconium Copper

    Lead-free Broken Slab FormConductivity PreservingGrain RefinerLow Concentration for Fine Addition Control
    Zirconium copper master alloy (90% Cu, 10% Zr) for grain refinement and property improvement in copper alloys. Broken slab form.
    Solidus filter
    1,782°F (972°C)
    Liquidus
    1,814°F (990°C)
    Density
    0.306 lbs/in³ (8.48 g/cm³)
    Primary Elements
    Cu · Zr
  • Product code: 5752

    1015 Babbitt ASTM B-23 Grade 7

    Arsenic HardenedASTM B-23 CompliantLead-BaseLow-Speed Bearing Grade
    Lead-base babbitt (10% Sn, 15% Sb, bal Pb, 0.45% As) per ASTM B-23 Grade 7 for low-speed bearing applications. 5-8 ingot.
    Solidus filter
    464°F (240°C)
    Liquidus
    514°F (268°C)
    Density
    0.35 lbs/in³ (9.7 g/cm³)
    Primary Elements
    As · Pb · Sb · Sn
  • Product code: 2451

    117 F, 47 C Low Melting Alloy

    Eutectic CompositionEven-Weight Cake FormExtremely Low Melting PointOptical Lens Blocking
    Five-component eutectic fusible alloy, 44.7% Bi / 22.6% Pb / 19.1% In / 8.3% Sn / 5.3% Cd. Melting point 117°F (47°C). Used for lens blocking and tooling aids.
    Solidus filter
    117°F (47°C)
    Liquidus
    117°F (47°C)
    Density
    0.32 lbs/in³ (8.86 | 8.9 g/cm³)
    Primary Elements
    Bi · Cd · In · Pb · Sn
  • Product code: 48712

    13% Zirconium Copper Alloy

    Lead-free 13% Zirconium Content40-50 Waffle FormCopper-Base Master AlloyGrain Refiner for Copper Alloys
    13% Zr copper-base master alloy in 40-50 waffle form. Used as grain refiner addition to copper alloys to improve mechanical properties.
    Solidus filter
    1,782°F (972°C)
    Liquidus
    1,950°F (1,066°C)
    Density
    0.313 lbs/in³ (8.66 g/cm³)
    Primary Elements
    Cu · Zr
  • Product code: 2491

    136 F, 58 C Low Melting Alloy

    Cadmium-FreeEutectic CompositionEven-Weight Cake FormLow Melting Point
    Cadmium-free eutectic fusible alloy, 49% Bi / 21% In / 18% Pb / 12% Sn. Melting point 136°F (58°C). Used for lens blocking, tooling, and fusible safety devices.
    Solidus filter
    136°F (58°C)
    Liquidus
    136°F (58°C)
    Density
    0.31 | 0.325 lbs/in³ (8.58 | 9.01 g/cm³)
    Primary Elements
    Bi · In · Pb · Sn
  • Product code: 48514

    15% Phosphor Copper

    Lead-free Clean Bright MeltFree-Flowing Shot FormMinimal Dross FormationMost Widely Used Copper Deoxidizer
    Phosphor copper deoxidizer (85% Cu, 15% P) — the most widely used copper alloy deoxidizer. Effectively removes oxygen with minimal dross. Shot and waffle forms.
    Solidus filter
    1,310°F (710°C)
    Liquidus
    1,310°F (710°C)
    Density
    0.283 lbs/in³ (7.85 g/cm³)
    Primary Elements
    Cu · P
  • Product code: 2502DS1C

    158-165 Degree F Low Melting Alloy Wire

    158F SolidusAntique and Wood Inlay ApplicationsLow-Temperature SolderNarrow Melting Range
    Bismuth-based Wood's Metal low melting alloy in solid wire form. Solidus 158F, liquidus 169F. Used as low-melting solder, metal inlays, and antique repair.
    Solidus filter
    158°F (70°C)
    Liquidus
    169°F (76°C)
    Density
    0.34 lbs/in³ (9.41 g/cm³)
    Primary Elements
    Bi · Cd · Pb · Sn

Showing 11–20 of 225 results