Jewelry Alloys

Alloys for jewelry and decorative casting, including lead-free pewter, white bronze, white brass, jewelers manganese bronze and spin-cast zinc alloys. Custom colors and compositions available on request.

Sort By:

Showing 10 of 17 products

  • Product code: 4907

    10% Cobalt Copper

    Lead-free Corrosion Resistance ImproverJewelry Alloy AdditionShot FormControlled Cobalt Addition
    Cobalt copper master alloy (90% Cu, 10% Co) for corrosion resistance improvement in copper alloys. Shot form for jewelry and foundry additions.
    Solidus
    1,994°F (1,090°C)
    Liquidus
    2,102°F (1,150°C)
    Density
    0.323 lbs/in³ (8.95 g/cm³)
    Primary Elements
    Cu · Co
  • Product code: 4001

    99.9% Electrolytic Copper

    Lead-free Maximum Electrical ConductivityJewelry and Art Casting GradeVirgin MaterialMultiple Forms
    High-purity electrolytic copper (99.95% Cu typical, 99.9% minimum) in polished and unpolished shot, polished and plain squares, and cathode forms for electrical, jewelry, and sculpture applications.
    Solidus
    1,950°F (1,066°C)
    Liquidus
    1,981°F (1,083°C)
    Density
    0.323 lbs/in³ (8.89 g/cm³)
    Primary Elements
    Cu
  • Product code: 46316

    Art Casters Brass

    Warm Yellow ColorExcellent CastabilityGold-Tone AppearanceJewelry Grade
    Proprietary warm-yellow brass for jewelry and art casting. Melting range 1,625–1,650°F. Gold-tone color. Forms: cubes, shot, bars, and ingots.
    Solidus
    1,625°F (885°C)
    Liquidus
    1,650°F (899°C)
    Density
    0.304 lbs/in³ (8.4 g/cm³)
    Primary Elements
    Cu · Zn · Pb · Si
  • Product code: 49817

    Belmont Special 2% Boron Copper

    Lead-free Eliminates Gas and PorosityNo Conductivity LossJewelry Alloy Grade1/2 and Down Polished Shot
    Belmont Special 2% boron copper master alloy in 1/2 and down polished shot. Eliminates gas and porosity in copper alloys without conductivity loss. Used in jewelry alloy production.
    Solidus
    1,850°F (1,010°C)
    Liquidus
    1,949°F (1,065°C)
    Density
    0.323 lbs/in³ (8.96 g/cm³)
    Primary Elements
    Cu · B
  • Product code: 4939

    Herculoy Silicon Bronze UNS C87610

    Lead-free CDA C87610 Excellent FluidityLow DrossingHigh DuctilityJewelry and Art Grade
    Herculoy silicon bronze (92% Cu, 4% Si, 4% Zn) per CDA C87610 for art, jewelry, and sculpture casting. Excellent fluidity, low drossing, high ductility.
    Solidus
    1,967°F (1,075°C)
    Liquidus
    1,985°F (1,085°C)
    Density
    0.302 lbs/in³ (8.4 g/cm³)
    Primary Elements
    Cu · Si · Zn
  • Product code: 4582

    Jewelers Manganese Bronze

    Unique Yellow Gold ColorJewelry Casting GradeExcellent CastabilityProprietary Formula
    Proprietary manganese bronze for jewelry casting with distinctive yellow gold color and excellent castability. Shot, cubes, bars, and ingot forms.
    Solidus
    1,580°F (860°C)
    Liquidus
    1,620°F (882°C)
    Density
    0.301 lbs/in³ (8.33 g/cm³)
    Primary Elements
    Cu · Zn · Al · Fe · Mn
  • Product code: 791NR8

    Lead Free Pewter (Britannia)

    Lead-free Britannia AlloySpin Cast Mold GradeFine Filigree DetailLead-Free Certified
    Lead-free Britannia pewter alloy for spin cast molds. Solidus 435-463F, liquidus 478-490F. Used for fashion jewelry with thin cross sections or fine filigree.
    Solidus
    435°F (224°C)
    Liquidus
    490°F (254°C)
    Density
    0.263 lbs/in³ (7.28 g/cm³)
    Primary Elements
    Sn · Sb · Cu
  • Product code: 791NB7

    Lead Free Pewter (Gravity Cast)

    Lead-free High Copper ContentOpen Face Gravity PourMaximum Mold DetailLead-Free Certified
    Lead-free high-copper pewter alloy. Used for open face, gravity pour, sand, and cast iron mold casting with maximum detail.
    Solidus
    471°F (244°C)
    Liquidus
    669°F (354°C)
    Density
    0.267 lbs/in³ (7.39 g/cm³)
    Primary Elements
    Sn · Sb · Cu
  • Product code: 798NENTB

    Lead Free Pewter with Bismuth

    Lead-free Less Than 50 ppm LeadHigh Purity Tin BaseThick Cross Section Spin CastingPolished Finish Grade
    High-purity tin-based lead-free pewter, less than 50 ppm lead. Solidus 515-635F, liquidus 465-485F. Used for spin cast rubber or silicone molds with thick cross sections.
    Solidus
    437°F (225°C)
    Liquidus
    442°F (228°C)
    Density
    0.265 lbs/in³ (7.33 g/cm³)
    Primary Elements
    Sn · Bi · Cu · Ag
  • Product code: 4951

    Silicon Bronze Everdur UNS C87300

    Lead-free CDA C87300 Excellent FluidityPatina CompatibleLow DrossingArt and Sculpture Grade
    Everdur silicon bronze (95% Cu, 4% Si, 1% Mn) per CDA C87300 for jewelry, sculpture, and marine casting. Excellent fluidity, low drossing, patina compatible.
    Solidus
    1,550°F (843°C)
    Liquidus
    1,780°F (971°C)
    Density
    0.302 lbs/in³ (8.36 g/cm³)
    Primary Elements
    Cu · Si · Mn

Showing 1–10 of 17 results