  • A390.1 Aluminum Alloy

    A390.1 Aluminum Alloy

    Hypereutectic Al-Si alloy (77.9% Al, 17% Si, 4.5% Cu, 0.6% Mg) with superior wear resistance and low thermal expansion. Engine...
    Lead-free
    Superior Wear Resistance Low Thermal Expansion Hypereutectic Si Engine Block Grade
    Solidus
    945°F (507°C)
    Liquidus
    1,200°F (649°C)
    Density
    0.099 lbs/in³ (2.73 g/cm³)
    Primary Elements
    Al · Si · Cu · Mg
    Nominal Composition
    0.6% Mg, 17% Si, 4.5% Cu, 77.9% Al
  • Nickel Treated Genuine Babbitt
    Product Code: 7886

    Nickel Treated Genuine Babbitt

    Nickel-treated tin-base babbitt (88% Sn, 8% Sb, 3.5% Cu, 0.5% Ni) with superior hardness, wear resistance, and corrosion resistance for...
    Lead-free
    Nickel-Treated Superior Wear Resistance Enhanced Corrosion Resistance Heavy-Duty Grade
    Solidus
    464°F (240°C)
    Liquidus
    680°F (360°C)
    Density
    0.267 lbs/in³ (7.4 g/cm³)
    Primary Elements
    Sn · Sb · Cu · Ni
    Nominal Composition
    3.5% Cu, 0.5% Ni, 8% Sb, 88% Sn