Multiple Supply Forms
Filter By
-
BASE Metal, 255 F, 124 C Low Melting Alloy
Bismuth-lead eutectic alloy (55.5% Bi, 44.5% Pb) melting at 255°F (124°C) for tube bending, work-holding, fusible safety devices, and low-temperature...Bismuth-lead eutectic alloy (55.5% Bi, 44.5% Pb) melting at 255°F (124°C) for tube bending, work-holding, fusible safety devices, and low-temperature soldering.Eutectic Sharp Melt at 255°F Tube Bending Mandrel Fill Work-Holding Grade Multiple Supply FormsSolidus255°F (124°C)Liquidus255°F (124°C)Density0.38 lbs/in³ (10.51 g/cm³)Primary ElementsBi · PbNominal Composition44.5% Pb, 55.5% BiBASE Metal, 255 F, 124 C Low Melting Alloy
Belmont Product Code: 2562Shipping Calculated at Checkout
Showing the single result