Master Alloy for Cr Additions

Filter By

Filters
Melting Point (Solidus), °F

Melting Point (Solidus), °F: 1967 — 1969

Density, lbs/in³

Density, lbs/in³: 0 — 1

Lead Free
See more See less
Custom Request
Can't find the right composition?
Get Expert Help

Sort By:

  • 10% Chrome Copper
    Product Code: 4906

    10% Chrome Copper

    Chrome copper master alloy (90% Cu, 10% Cr) for introducing chromium into copper alloys to improve corrosion resistance and conductivity....
    Lead-free
    Master Alloy for Cr Additions Corrosion Resistance Improver Grain Refiner Controlled Addition
    Solidus
    1,969°F (1,076°C)
    Liquidus
    2,444°F (1,340°C)
    Density
    0.315 lbs/in³ (8.72 g/cm³)
    Primary Elements
    Cu · Cr
    Nominal Composition
    10% Cr, 90% Cu
  • Chrome Copper UNS C81500
    Product Code: 4989

    Chrome Copper UNS C81500

    Chrome copper (98.7% Cu, 1.3% Cr) per CDA C81500. High conductivity high-strength master alloy for chromium additions. Solidus 1967F liquidus...
    Lead-free
    High Conductivity Precipitation Hardenable Master Alloy for Cr Additions Elevated Temperature Strength
    Solidus
    1,967°F (1,075°C)
    Liquidus
    1,985°F (1,085°C)
    Density
    0.319 lbs/in³ (8.82 g/cm³)
    Primary Elements
    Cu · Cr
    Nominal Composition
    1.3% Cr, 98.7% Cu

Showing all 2 results