Jackson Wheeler Tuftin Line

Filter By

Filters
Melting Point (Solidus), °F

Melting Point (Solidus), °F: 464 — 464

Density, lbs/in³

Density, lbs/in³: 0 — 1

Lead Free
  • There are no filter terms yet
  • There are no filter terms yet
See more See less
Custom Request
Can't find the right composition?
Get Expert Help

Sort By:

  • Tuftin No. 73 Nickel Alloy
    Product Code: E5

    Tuftin No. 73 Nickel Alloy

    Proprietary tin-base Babbitt with nickel additions for enhanced strength. Available as ingot.
    Lead-free
    Enhanced Strength Industrial Bearing Grade Jackson Wheeler Tuftin Line Nickel-Modified Tin-Base Babbitt
    Solidus
    464°F (240°C)
    Liquidus
    824°F (440°C)
    Density
    0.269 lbs/in³ (7.45 g/cm³)
    Primary Elements
    Cu, Ni, Sb, Sn, Te
    Nominal Composition
    Proprietary
    Shapes
    Bars, Wire

Showing the single result