  • Tuftex Duratex Alloy
    Product Code: J1

    Tuftex Duratex Alloy

    Proprietary lead-base alloy with nickel addition for increased hardness. Available as ingot.
    Higher Load Capacity Than Standard Lead Babbitt Increased Hardness Jackson Wheeler Proprietary Nickel-Modified Lead-Base Babbitt
    Solidus
    462°F (239°C)
    Liquidus
    487°F (253°C)
    Density
    0.361 lbs/in³ (10 g/cm³)
    Primary Elements
    Cu, Ni, Pb, Sb, Sn
    Nominal Composition
    Proprietary
    Shapes
    Cakes