  • A357.2 Aluminum Alloy

    A357.2 Aluminum Alloy

    High-strength Al-Si-Mg casting alloy (92.2% Al, 7% Si, 0.6% Mg) with excellent pressure tightness. Heat treatable. 30 lb ingot.
    Lead-free
    High Strength Excellent Pressure Tightness Heat Treatable
    Solidus
    1,035°F (557°C)
    Liquidus
    1,135°F (613°C)
    Density
    0.097 lbs/in³ (2.68 g/cm³)
    Primary Elements
    Al · Si · Mg
    Nominal Composition
    0.6% Mg, 7% Si, 92.2%Al, Bal