Corrosion Resistance Improver

Filter By

Filters
Melting Point (Solidus), °F

Melting Point (Solidus), °F: 1969 — 1994

Density, lbs/in³

Density, lbs/in³: 0 — 1

Lead Free
  • There are no filter terms yet
  • There are no filter terms yet
See more See less
Custom Request
Can't find the right composition?
Get Expert Help

Sort By:

  • 10% Chrome Copper
    Product Code: 4906

    10% Chrome Copper

    Chrome copper master alloy (90% Cu, 10% Cr) for introducing chromium into copper alloys to improve corrosion resistance and conductivity....
    Lead-free
    Controlled Addition Corrosion Resistance Improver Grain Refiner Master Alloy for Cr Additions
    Solidus
    1,969°F (1,076°C)
    Liquidus
    2,444°F (1,340°C)
    Density
    0.315 lbs/in³ (8.72 g/cm³)
    Primary Elements
    Cr, Cu
    Nominal Composition
    10% Cr, 90% Cu
    Shapes
    Ingot
  • 10% Cobalt Copper
    Product Code: 4907

    10% Cobalt Copper

    Cobalt copper master alloy (90% Cu, 10% Co) for corrosion resistance improvement in copper alloys. Shot form for jewelry and...
    Lead-free
    Controlled Cobalt Addition Corrosion Resistance Improver Jewelry Alloy Addition Jewelry and Foundry Grade
    Solidus
    1,994°F (1,090°C)
    Liquidus
    2,102°F (1,150°C)
    Density
    0.323 lbs/in³ (8.95 g/cm³)
    Primary Elements
    Co, Cu
    Nominal Composition
    10% Co, 90% Cu
    Shapes
    Shot

Showing all 2 results