  • 20% Chrome Aluminum
    Product Code: 18012

    20% Chrome Aluminum

    Al-Cr master alloy (80% Al, 20% Cr) for grain structure control in 5xxx and 7xxx series aluminum alloys. Suppresses recrystallization....
    Lead-free
    Grain Structure Control Recrystallization Suppression Stress-Corrosion Resistance Aerospace Grade
    Solidus
    1,220°F (660°C)
    Liquidus
    1,920°F (1,049°C)
    Density
    0.111 lbs/in³ (3.08 g/cm³)
    Primary Elements
    Al · Cr
    Nominal Composition
    20% Cr, 80% Al
  • 5% Lithium Aluminum
    Product Code: 19515

    5% Lithium Aluminum

    Al-Li master alloy (95% Al, 5% Li) for oxidation control in Mg-bearing alloys and density reduction in aerospace applications. Ingot...
    Lead-free
    Oxidation Control Density Reduction Modulus Increase Aerospace Grade
    Solidus
    1,112°F (600°C)
    Liquidus
    1,185°F (641°C)
    Density
    0.083 lbs/in³ (2.3 g/cm³)
    Primary Elements
    Al · Li
    Nominal Composition
    5% Li, 95% Al
  • A201.1 Aluminum Alloy

    A201.1 Aluminum Alloy

    Ultra-high-strength Al-Cu-Ag alloy (94% Al, 4.5% Cu, 0.7% Ag) delivering nearly double the tensile strength of 300-series alloys. Aerospace grade.
    Lead-free
    Ultra-High Tensile Strength Heat Treatable Aerospace Grade High Fracture Toughness
    Solidus
    1,005°F (541°C)
    Liquidus
    1,205°F (652°C)
    Density
    0.101 lbs/in³ (2.8 g/cm³)
    Primary Elements
    Al · Cu · Ag
    Nominal Composition
    0.7% Ag, 4.5% Cu, 94% Al, Bal
  • A203.2 Aluminum Alloy

    A203.2 Aluminum Alloy

    High-strength Al-Cu-Ni casting alloy (92.35% Al, 5% Cu, 1.5% Ni) with elevated-temperature stability. Aerospace and structural grade. 3-16 ingot.
    Lead-free
    Ultra-High Strength Enhanced Elevated-Temperature Stability Aerospace Grade
    Solidus
    995°F (535°C)
    Liquidus
    1,185°F (641°C)
    Density
    0.101 lbs/in³ (2.79 g/cm³)
    Primary Elements
    Al · Cu · Ni
    Nominal Composition
    1.5% Ni, 5% Cu, 92.35% Al, Bal
  • C355.2 Aluminum Alloy

    C355.2 Aluminum Alloy

    High-purity Al-Si-Cu-Mg casting alloy (93% Al, 5% Si, 1% Cu) with superior pressure tightness and fatigue strength. Aerospace grade. 30...
    Lead-free
    Superior Pressure Tightness High Fatigue Strength High-Purity Grade Aerospace Grade
    Solidus
    1,015°F (546°C)
    Liquidus
    1,150°F (621°C)
    Density
    0.098 lbs/in³ (2.71 g/cm³)
    Primary Elements
    Al · Si · Cu · Mg
    Nominal Composition
    1% Cu, 5% Si, 93% Al, Bal
  • C357.2 Aluminum Alloy

    C357.2 Aluminum Alloy

    High-purity Al-Si-Mg casting alloy (92.22% Al, 7% Si, 0.6% Mg) with exceptional fracture toughness. Safety-critical aerospace grade. ~35 lb ingot.
    Lead-free
    High-Purity Grade Exceptional Fracture Toughness Aerospace Grade Superior Corrosion Resistance
    Solidus
    1,035°F (557°C)
    Liquidus
    1,135°F (613°C)
    Density
    0.097 lbs/in³ (2.68 g/cm³)
    Primary Elements
    Al · Si · Mg
    Nominal Composition
    0.6% Mg, 7% Si, 92.22% Al, Bal