  • 1015 Babbitt ASTM B-23 Grade 7
    Product Code: 5752

    1015 Babbitt ASTM B-23 Grade 7

    Lead-base babbitt (10% Sn, 15% Sb, bal Pb, 0.45% As) per ASTM B-23 Grade 7 for low-speed bearing applications. 5-8...
    Arsenic Hardened ASTM B-23 Compliant Lead-Base Low-Speed Bearing Grade
    Solidus
    464°F (240°C)
    Liquidus
    514°F (268°C)
    Density
    0.35 lbs/in³ (9.7 g/cm³)
    Primary Elements
    As, Pb, Sb, Sn
    Nominal Composition
    0.45% As, 10% Sn, 15% Sb, Bal Pb
    Shapes
    Ingot