Sort By:

  • Special 92% Tin Pewter
    Product Code: 7924

    Special 92% Tin Pewter

    Tin-lead-antimony pewter (92% Sn, 4% Pb, 4% Sb) with excellent casting characteristics for figurines and models with heavy sections. 5-6...
    Better Fill than Lead-Free Britannia Figurine and Model Grade High Tin Base with Lead Pressure Tightness Superior Casting in Heavy Sections
    Solidus
    430°F (221°C)
    Liquidus
    443°F (228°C)
    Density
    0.269 lbs/in³ (7.45 g/cm³)
    Primary Elements
    Pb, Sb, Sn
    Nominal Composition
    4% Pb, 4% Sb, 92% Sn
    Shapes
    Ingot
  • Tuftin No. 73 Nickel Alloy
    Product Code: E5

    Tuftin No. 73 Nickel Alloy

    Proprietary tin-base Babbitt with nickel additions for enhanced strength. Available as ingot.
    Lead-free
    Enhanced Strength Industrial Bearing Grade Jackson Wheeler Tuftin Line Nickel-Modified Tin-Base Babbitt
    Solidus
    464°F (240°C)
    Liquidus
    824°F (440°C)
    Density
    0.269 lbs/in³ (7.45 g/cm³)
    Primary Elements
    Cu, Ni, Sb, Sn, Te
    Nominal Composition
    Proprietary
    Shapes
    Bars, Wire