  • 20% Magnesium Copper Alloy
    Product Code: 4800

    20% Magnesium Copper Alloy

    Magnesium copper master alloy (80% Cu, 20% Mg) for deoxidizing and degassing nickel and copper alloy melts. Broken slab form.
    Lead-free
    Degasser Deoxidizer Nickel Alloy Treatment Sulfur Scavenger
    Solidus
    1,346°F (730°C)
    Liquidus
    1,746°F (952°C)
    Density
    0.267 lbs/in³ (7.4 g/cm³)
    Primary Elements
    Cu, Mg
    Nominal Composition
    20% Mg, 80% Cu
    Shapes
    Lumps, Slabs
  • Heavy Duty Babbitt ASTM B-23 Grade 3
    Product Code: 7852

    Heavy Duty Babbitt ASTM B-23 Grade 3

    Heavy-duty tin-base babbitt (84% Sn, 8% Sb, 8% Cu) per ASTM B-23 Grade 3 for high-load bearing applications. Ingot and...
    ASTM B-23 Compliant Field Repair Grade Furnace Pouring Grade Hardest Tin-Base Grade
    Solidus
    464°F (240°C)
    Liquidus
    792°F (422°C)
    Density
    0.267 lbs/in³ (7.4 g/cm³)
    Primary Elements
    Cu, Sb, Sn
    Nominal Composition
    8% Cu, 8% Sb, 84% Sn,  
    Shapes
    Ingot, Wire
  • Nickel Treated Genuine Babbitt
    Product Code: 7886

    Nickel Treated Genuine Babbitt

    Nickel-treated tin-base babbitt (88% Sn, 8% Sb, 3.5% Cu, 0.5% Ni) with superior hardness, wear resistance, and corrosion resistance for...
    Lead-free
    Enhanced Corrosion Resistance Heavy-Duty Grade Nickel-Treated Superior Wear Resistance
    Solidus
    464°F (240°C)
    Liquidus
    680°F (360°C)
    Density
    0.267 lbs/in³ (7.4 g/cm³)
    Primary Elements
    Cu, Ni, Sb, Sn
    Nominal Composition
    3.5% Cu, 0.5% Ni, 8% Sb, 88% Sn
    Shapes
    Ingot, Wire

Showing all 3 results