  • CAST Metal, 281-338 F, 138-170 C Low Melting Alloy
    Product Code: 2405

    CAST Metal, 281-338 F, 138-170 C Low Melting Alloy

    Bismuth-tin non-eutectic alloy (40% Bi, 60% Sn) with 281-338°F (138-170°C) melting range for lost-pattern casting, proof casting, and low-temperature sealing.
    Lead-free
    Lost-Pattern Casting Substitute Lowest Density in Low Melt Range Proof Casting Grade Minimal Dimensional Change
    Solidus
    281°F (138°C)
    Liquidus
    338°F (170°C)
    Density
    0.3 lbs/in³ (8.4 g/cm³)
    Primary Elements
    Bi · Sn
    Nominal Composition
    40% Bi, 60% Sn
  • TRU Alloy, 281 F, 138 C Eutectic Low Melting Alloy
    Product Code: 2581

    TRU Alloy, 281 F, 138 C Eutectic Low Melting Alloy

    Binary eutectic fusible alloy, 58% Bi / 42% Sn. Melting point 281°F (138°C). Lead-free. Used for jet engine blade fixturing,...
    Lead-free
    Eutectic Composition Minimal Volume Change on Solidification Lead-Free Aerospace Fixturing
    Solidus
    281°F (138°C)
    Liquidus
    281°F (138°C)
    Density
    0.309 lbs/in³ (8.72 g/cm³)
    Primary Elements
    Bi · Sn
    Nominal Composition
    42% Sn, 58% Bi